Material No.: N 08800
Description
|
| ||||||||||||||||||||||||
| |||||||||||||||||||||||||
Chemical Composition
| C | Si | S | Ti | Cu | Mn | Fe | Cr | Ni | Al | P | ||
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| N 08800 | Min % | 0,15 | 39,5 | 19,0 | 30,0 | 0,15 | ||||||
| Max % | 0,10 | 1,0 | 0,015 | 0,60 | 0,75 | 1,50 | 23,0 | 35,0 | 0,60 | |||
| ASTM B 407 (N 08800-Alloy 800) | ||||||||||||
| 1.4876 | Min % | 0,15 | 19,00 | 30,00 | 0,15 | |||||||
| Max % | 0,12 | 1,00 | 0,015 | 0,60 | 2,0 | 23,00 | 34,00 | 0,60 | 0,030 | |||
| (Key to steel 2010) | ||||||||||||
| alloy 800 | Min % | |||||||||||
| Max % | ||||||||||||
Physical properties
| Property | Value |
|---|---|
| Density: lb//in3 | 0,287 |
| Hardness: HB30 | <=192 |
| permeability by 20°C | 1,01 |
| magnetizable | no |
| elasticity modulus (N/mm2) /ksi | 194 / 28,1 |
| Temperature T °C/F (°C/F) | Specific heat J / kgK (Btu / lb °F) | Thermal conductivity W/mK (Btu·in / ft2·h·°F) | Electric resistance µΩ · cm (Ω circ mill / ft) | Modulus of elasticity kN/mm2 (103 ksi) | Expansion rate from 70°F bis T 10-6 / K (10-6 / °F) |
|---|---|---|---|---|---|
| 20 / 68 | 472 (--) | 11,5 (--) | 101 (--) | 194 (--) | 12 (--) |
| 100 / 212 | 501 (--) | 13,1 (--) | 104 (--) | 189 (--) | 15,1 (--) |
| 200 / 392 | 525 (--) | 14,8 (--) | 108 (--) | 183 (--) | 15,7 (--) |
| 300 / 572 | 532 (--) | 16,4 (--) | 112 (--) | 177 (--) | 16,2 (--) |
| 400 / 752 | 555 (--) | 18,1 (--) | 115 (--) | 170 (--) | 16,6 (--) |
| 500 / 932 | 582 (--) | 19,6 (--) | 118 (--) | 163 (--) | 17,0 (--) |
| 600 / 1112 | 604 (--) | 21,2 (--) | 120 (--) | 156 (--) | 17,4 (--) |
| 800 /1472 | 609 (--) | 24,3 (--) | 124 (--) | 141 (--) | 18,0 (--) |
| 1000 / 1832 | 641 (--) | 27,3 (--) | 127 (--) | 127 (--) | 18,6 (--) |
| Temp. | Creep strain limit | Creep strain limit | Creep rupture strength | Creep rupture strength | Creep rupture strength |
|---|---|---|---|---|---|
| 1000 h | °C/°F | Mpa/ksi | |||
| 650 / 1202 | 165 / 23,9 | ||||
| 705 / 1300 | 105 / 15,2 | ||||
| 870 /1600 | 32 / 4,7 | ||||
| 980 /1800 | 14 / 2,0 |
| Temperature | Yield strength in high temperatures | Yield strength in high temperatures | Tensile strenght in high temperatures |
|---|---|---|---|
| °C / °F | Rp 1,0 | Rp 0,2 | Rm | N/mm2 / ksi | N/mm2 /ksi | N/mm2 /ksi |
| 20 / 68 | 200 / 29 | 170 / 24,6 | 450 / 65,2 |
| 100 / 212 | 160 / 23,2 | 140 / 20,3 | 400 / 58,0 |
| 300 / 572 | 115 / 16,6 | 95 / 13,7 | 390 / 56,5 |
| 500 / 932 | 100 / 15,4 | 80 / 11,6 | 360 / 52,2 |
| 600 / 1112 | 95 / 13,7 | 75 / 10,9 | 300 / 43,5 |
| ksi value calculated | |||
Mechanical properties (20°C / 68°F)
| 1 %Yield strength Rp 1,0 Mpa(ksi | 200 / 29 | ||
|---|---|---|---|
| tensile elastic limit (Mpa) /ksi | >=170 />=24,6 | ||
| Tensile strenght Rm (Mpa) | 450-680 | ||
| Elongation A5 (%) | >=30 >=35 | quer längs | |
| impact work KV(ISO-V)/Jcm2 | >=150 >=100 | längs quer | |
Temparature information
| Application area | ||
|---|---|---|
| Operation temperature | ºF to 1112 ºF | air to 2012°F |
| Explanation report | soft-annealed : resistant to scaling by air to 2012 °F | |
| Solution heat treatment | ||
|---|---|---|
| Working temperature | 1922 ºF to 2102 ºF | |
| Explanation report | cooling down Water/air | |
| soft-annealed | ||
|---|---|---|
| Working temperature | 1688 ºF to 2552 ºF | |
| Solution heat treatment | ||
|---|---|---|
| Working temperature | 1832 ºF to 2282 ºF | |
Standards / information
| Standards | Desciption |
|---|---|
| ASTM A 312 | Standard Specification for Seamless and welded austenitic stainless steel pipes |
| ASTM B 163 | Standard Specifications for seamless nickel and nickel alloy condensers and heat-exchanger tubes |
| ASTM B 407 | Standard Specification for Nickel-Iron-Chromium Alloy Seamless Pipe and Tube |
| ASTM B 408 | Standard Specification for Nickel-Iron-Chromium Alloy Rod and Bar |
| ASTM B 409 | Standard Specification for Nickel-Iron-Cromium Alloy metal sheets |
| DIN EN 10297-2 (02/2006) | seamless circular steel pipes for machine construction and general technical applications, stainless steel |
| SEW 310 (08/1992) | physical properties of steel |
| SEW 470 (02/1976) | heat-resisting rolled and forged steels |
| VdTÜV-Werkstoffblatt 412 | rolled/forged steel, X10NiCrAlTi 32-20, material-nr. 1.4876; sheet metal, ribbon, rod steel, forging, seamless pipe |
| VdTÜV WBL-412 | rolled / forged steel material-nr.1.4876 (12/2009) |
Process information
| Chip removing process | process in annealed state, due to cold work hardening low cutting speed keep constant cutting tool contact |
|---|
| Welding | |
|---|---|
| - Material classification acc. CEN ISO/TR 15608 | 8,2 |
| - Type | well weldable all methods of welding |
| - Add. material | 2.4806/2.4807 |
Main fields of application
| Details of application | scaling resistant in air up to 2012°F corrosion and heat resistant |
|---|---|
| Certifications | Nace MR 01-75 |
| Einsatzgebiete kleiner 600°C | |
| industral furnace engineering | |
| Apparatus engineering | |
| crude oil |
Range of products
| Product type | Product |
|---|---|
| Plates / Sheets | plates/sheets plate/sheet cuts |
| Fittings | welded elbows welded reductions Welded T-pieces seamless elbows seamless reductions seamless T-pieces |
| Flanges / Collars / Flared tube ends | various flanges (weld neck flange,blind flange etc.) |
| Pipes / Tubes | welded pipes/tubes seamless pipes/tubes |
| Bar steel | flat steel round bar steel |
Liability exclusion