Material No.: K 90941
Description
|
|
Chemical Composition
| C | Mn | P | Si | Cr | Mo | S | Cu | Al | Fe | ||
|---|---|---|---|---|---|---|---|---|---|---|---|
| K 90941 | Min % | 0,30 | 0,50 | 8,00 | 0,90 | ||||||
| Max % | 0,15 | 0,60 | 0,030 | 1,00 | 10,00 | 1,10 | 0,030 | ||||
| 1.7386 | Min % | 0,08 | 0,30 | 0,25 | 8,00 | 0,90 | |||||
| Max % | 0,15 | 0,60 | 0,025 | 1.00 | 10,00 | 1,10 | 0,20 | 0,30 | 0,040 | ||
| (Key to Steel 2010) | |||||||||||
Physical properties
| Property | Value |
|---|---|
| Density: kg/dm3 | 7,77 |
| Hardness: (HB) | --- |
| Temperature T °C/F (°C/F) | Specific heat J / kgK (Btu / lb °F) | Thermal conductivity W/mK (Btu·in / ft2·h·°F) | Electric resistance µΩ · cm (Ω circ mill / ft) | Modulus of elasticity kN/mm2 (103 ksi) | Expansion rate from 70°F bis T 10-6 / K (10-6 / °F) |
|---|---|---|---|---|---|
| 20/ | 21/() | 217 | |||
| 100/ | 23/() | ||||
| 200/ | 24/() | ||||
| 300/ | 26/() | ||||
| 400/ | 27/() | ||||
| 500/ | 28/() | ||||
| 600/ | 29/() |
| Temp. | Creep strain limit | Creep strain limit | Creep rupture strength | Creep rupture strength | Creep rupture strength |
|---|---|---|---|---|---|
| °C/°F | 100 000 h | 200 000H | °C/°F | Mpa / ksi | Mpa /ksi |
| 400 / 752 | |||||
| 450 / 842 | 276 / 40,0 | 259 / 37,5 | |||
| 480 / 896 | 211 / 30,6 | 196 / 28,4 | |||
| 500 / 932 | 174 / 25,2 | 160 /23,2 | |||
| 550 / 1022 | 92 / 13,3 | 80 / 11,6 | |||
| ksi value calculated | |||||
Mechanical properties (20°C / 68°F)
| Dehngrenze | 220-390 /31,9-56,5 | ||
|---|---|---|---|
| Dehngrenze | |||
| Zugfestigkeit | 590-750 /85,5-108,7 | ||
| Bruchdehnung | 20 % /18 % | ||
| Schlagarbeit ISO-V | > 40J | lengthwise | |
| (Mittelwert von 3 Proben) | |||
Temparature information
| Application area | ||
|---|---|---|
| Operation temperature | 14 ºF to 1022 ºF | |
| hardness | ||
|---|---|---|
| Working temperature | 1634 ºF to 1742 ºF | |
| Explanation report | cooldown: air/oil | |
| Solution heat treatment | ||
|---|---|---|
| Working temperature | 1472 ºF to 2012 ºF | |
| annealing | ||
|---|---|---|
| Working temperature | 1328 ºF to 1472 ºF | |
| Explanation report | cooldown: air | |
| Normalizing | ||
|---|---|---|
| Working temperature | 1634 ºF to 1742 ºF | |
| Heat treating | ||
|---|---|---|
| Working temperature | 1562 ºF to 2012 ºF | |
Standards / information
| Standards | Desciption |
|---|---|
| ASTM A 213 | Standard Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler,Superheater,and Heat-Exchanger Tubes |
| ASTM B 335 | Standard Specification for Nickel-Molybdenium Alloy rods |
Process information
| Welding | |
|---|---|
| - Type | manual arc welding |
| - Add. material | same type material |
Main fields of application
| Details of application | |
|---|---|
| Certifications | |
| Power engineering | Überhitzerrohre Sammler |
Range of products
| Product type | Product |
|---|---|
| Plates / Sheets | plates/sheets plate/sheet cuts |
| Fittings | welded elbows welded reductions Welded T-pieces seamless elbows seamless reductions seamless T-pieces Other Fittings a.o. Weldolets, Nipples |
| Pipes / Tubes | welded pipes/tubes seamless pipes/tubes |